{"_buckets": {"deposit": "41ceed88-87e6-4797-b068-d72a0517d208"}, "_deposit": {"id": "4171", "owners": [], "pid": {"revision_id": 0, "type": "depid", "value": "4171"}, "status": "published"}, "_oai": {"id": "oai:niigata-u.repo.nii.ac.jp:00004171", "sets": ["454", "425"]}, "item_5_alternative_title_1": {"attribute_name": "その他のタイトル", "attribute_value_mlt": [{"subitem_alternative_title": "Solid State Welding between CPTi and AZ31B Magnesium Alloy Using a Rotating Probe with Thread"}]}, "item_5_biblio_info_6": {"attribute_name": "書誌情報", "attribute_value_mlt": [{"bibliographicIssueDates": {"bibliographicIssueDate": "2007", "bibliographicIssueDateType": "Issued"}, "bibliographicIssueNumber": "2", "bibliographicPageEnd": "393", "bibliographicPageStart": "386", "bibliographicVolumeNumber": "25", "bibliographic_titles": [{"bibliographic_title": "溶接学会論文集"}, {"bibliographic_title": "溶接学会論文集", "bibliographic_titleLang": "en"}]}]}, "item_5_description_4": {"attribute_name": "抄録", "attribute_value_mlt": [{"subitem_description": "This paper describes a butt-welding of AZ31B magnesium alloy plate to commercially pure titanium (CPTi) plate by the solid state welding using a rotating probe with a thread, The effect of the right-hand and left-hand thread on the tensile strength and microstructure was investigated. The following results were obtained in this study. The probe with a thread increased the tensile strength of a joint by about 79% or less compared with without a thread. There were little differences in the maximum tensile strength of the joints made by the right-hand thread and the left-hand thread. Using the probe without a thread, the fragments of CPTi were produced in a continuous form, but using the probe with a thread. the fine fragments of CPTi tended to scatter in Mg alloy matrix. The increase in the tensile strength of the joints using the probe with a thread was considered to be due to the sufficient plastic flow of Mg alloy caused by the fine fragments of CPTi scattered in Mg alloy matrix. However, the tensile strength of the joint was lower than that of the parent material and the fracture path occurred around the interface. X-ray diffraction analysis revealed a deformation texture with the (002) basal plane near the interface of the magnesium side. It seems that both of the decrease in Al concentration in the Mg alloy and the formation of the deformation texture with the (002) basal plane caused the tensile strength lower, compared with parent material.", "subitem_description_type": "Abstract"}]}, "item_5_full_name_3": {"attribute_name": "著者別名", "attribute_value_mlt": [{"nameIdentifiers": [{"nameIdentifier": "47855", "nameIdentifierScheme": "WEKO"}], "names": [{"name": "Tanabe, Hiroshi"}]}, {"nameIdentifiers": [{"nameIdentifier": "47856", "nameIdentifierScheme": "WEKO"}], "names": [{"name": "Watanabe, Takehiko"}]}, {"nameIdentifiers": [{"nameIdentifier": "47857", "nameIdentifierScheme": "WEKO"}], "names": [{"name": "Yoshida, Ryou"}]}, {"nameIdentifiers": [{"nameIdentifier": "47858", "nameIdentifierScheme": "WEKO"}], "names": [{"name": "Yanagisawa, Atsushi"}]}]}, "item_5_publisher_7": {"attribute_name": "出版者", "attribute_value_mlt": [{"subitem_publisher": "溶接学会"}]}, "item_5_select_19": {"attribute_name": "著者版フラグ", "attribute_value_mlt": [{"subitem_select_item": "publisher"}]}, "item_5_source_id_11": {"attribute_name": "書誌レコードID", "attribute_value_mlt": [{"subitem_source_identifier": "AN1005067X", "subitem_source_identifier_type": "NCID"}]}, "item_5_source_id_9": {"attribute_name": "ISSN", "attribute_value_mlt": [{"subitem_source_identifier": "02884771", "subitem_source_identifier_type": "ISSN"}]}, "item_creator": {"attribute_name": "著者", "attribute_type": "creator", "attribute_value_mlt": [{"creatorNames": [{"creatorName": "田辺, 寛"}], "nameIdentifiers": [{"nameIdentifier": "47851", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "渡辺, 健彦"}], "nameIdentifiers": [{"nameIdentifier": "47852", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "吉田, 亮"}], "nameIdentifiers": [{"nameIdentifier": "47853", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "柳沢, 敦"}], "nameIdentifiers": [{"nameIdentifier": "47854", "nameIdentifierScheme": "WEKO"}]}]}, "item_files": {"attribute_name": "ファイル情報", "attribute_type": "file", "attribute_value_mlt": [{"accessrole": "open_date", "date": [{"dateType": "Available", "dateValue": "2019-07-30"}], "displaytype": "detail", "download_preview_message": "", "file_order": 0, "filename": "06_0005.pdf", "filesize": [{"value": "775.7 kB"}], "format": "application/pdf", "future_date_message": "", "is_thumbnail": false, "licensetype": "license_free", "mimetype": "application/pdf", "size": 775700.0, "url": {"label": "06_0005.pdf", "url": "https://niigata-u.repo.nii.ac.jp/record/4171/files/06_0005.pdf"}, "version_id": "c65bf0bc-ef75-416b-aeec-4501c169d43f"}]}, "item_keyword": {"attribute_name": "キーワード", "attribute_value_mlt": [{"subitem_subject": "Joining of dissimilar metals", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Butt joint", "subitem_subject_scheme": "Other"}, {"subitem_subject": "CPTi", "subitem_subject_scheme": "Other"}, {"subitem_subject": "AZ31B Magnesium alloy", "subitem_subject_scheme": "Other"}, {"subitem_subject": "FSW", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Tensile Strength", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Thread", "subitem_subject_scheme": "Other"}]}, "item_language": {"attribute_name": "言語", "attribute_value_mlt": [{"subitem_language": "jpn"}]}, "item_resource_type": {"attribute_name": "資源タイプ", "attribute_value_mlt": [{"resourcetype": "journal article", "resourceuri": "http://purl.org/coar/resource_type/c_6501"}]}, "item_title": "ねじ付回転プローブによる工業用純チタンとAZ31Bマグネシウム合金の固相接合", "item_titles": {"attribute_name": "タイトル", "attribute_value_mlt": [{"subitem_title": "ねじ付回転プローブによる工業用純チタンとAZ31Bマグネシウム合金の固相接合"}, {"subitem_title": "ねじ付回転プローブによる工業用純チタンとAZ31Bマグネシウム合金の固相接合", "subitem_title_language": "en"}]}, "item_type_id": "5", "owner": "1", "path": ["454", "425"], "permalink_uri": "http://hdl.handle.net/10191/6287", "pubdate": {"attribute_name": "公開日", "attribute_value": "2008-04-23"}, "publish_date": "2008-04-23", "publish_status": "0", "recid": "4171", "relation": {}, "relation_version_is_last": true, "title": ["ねじ付回転プローブによる工業用純チタンとAZ31Bマグネシウム合金の固相接合"], "weko_shared_id": null}
ねじ付回転プローブによる工業用純チタンとAZ31Bマグネシウム合金の固相接合
http://hdl.handle.net/10191/6287
http://hdl.handle.net/10191/6287bb5a9fef-6c21-4640-ad30-bcfb1c59b3dc
名前 / ファイル | ライセンス | アクション |
---|---|---|
![]() |
|
Item type | 学術雑誌論文 / Journal Article(1) | |||||
---|---|---|---|---|---|---|
公開日 | 2008-04-23 | |||||
タイトル | ||||||
タイトル | ねじ付回転プローブによる工業用純チタンとAZ31Bマグネシウム合金の固相接合 | |||||
タイトル | ||||||
言語 | en | |||||
タイトル | ねじ付回転プローブによる工業用純チタンとAZ31Bマグネシウム合金の固相接合 | |||||
言語 | ||||||
言語 | jpn | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | Joining of dissimilar metals | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | Butt joint | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | CPTi | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | AZ31B Magnesium alloy | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | FSW | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | Tensile Strength | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | Thread | |||||
資源タイプ | ||||||
資源 | http://purl.org/coar/resource_type/c_6501 | |||||
タイプ | journal article | |||||
その他のタイトル | ||||||
その他のタイトル | Solid State Welding between CPTi and AZ31B Magnesium Alloy Using a Rotating Probe with Thread | |||||
著者 |
田辺, 寛
× 田辺, 寛× 渡辺, 健彦× 吉田, 亮× 柳沢, 敦 |
|||||
著者別名 | ||||||
識別子 | 47855 | |||||
識別子Scheme | WEKO | |||||
姓名 | Tanabe, Hiroshi | |||||
著者別名 | ||||||
識別子 | 47856 | |||||
識別子Scheme | WEKO | |||||
姓名 | Watanabe, Takehiko | |||||
著者別名 | ||||||
識別子 | 47857 | |||||
識別子Scheme | WEKO | |||||
姓名 | Yoshida, Ryou | |||||
著者別名 | ||||||
識別子 | 47858 | |||||
識別子Scheme | WEKO | |||||
姓名 | Yanagisawa, Atsushi | |||||
抄録 | ||||||
内容記述タイプ | Abstract | |||||
内容記述 | This paper describes a butt-welding of AZ31B magnesium alloy plate to commercially pure titanium (CPTi) plate by the solid state welding using a rotating probe with a thread, The effect of the right-hand and left-hand thread on the tensile strength and microstructure was investigated. The following results were obtained in this study. The probe with a thread increased the tensile strength of a joint by about 79% or less compared with without a thread. There were little differences in the maximum tensile strength of the joints made by the right-hand thread and the left-hand thread. Using the probe without a thread, the fragments of CPTi were produced in a continuous form, but using the probe with a thread. the fine fragments of CPTi tended to scatter in Mg alloy matrix. The increase in the tensile strength of the joints using the probe with a thread was considered to be due to the sufficient plastic flow of Mg alloy caused by the fine fragments of CPTi scattered in Mg alloy matrix. However, the tensile strength of the joint was lower than that of the parent material and the fracture path occurred around the interface. X-ray diffraction analysis revealed a deformation texture with the (002) basal plane near the interface of the magnesium side. It seems that both of the decrease in Al concentration in the Mg alloy and the formation of the deformation texture with the (002) basal plane caused the tensile strength lower, compared with parent material. | |||||
書誌情報 |
溶接学会論文集 en : 溶接学会論文集 巻 25, 号 2, p. 386-393, 発行日 2007 |
|||||
出版者 | ||||||
出版者 | 溶接学会 | |||||
ISSN | ||||||
収録物識別子タイプ | ISSN | |||||
収録物識別子 | 02884771 | |||||
書誌レコードID | ||||||
収録物識別子タイプ | NCID | |||||
収録物識別子 | AN1005067X | |||||
著者版フラグ | ||||||
値 | publisher |