@article{oai:niigata-u.repo.nii.ac.jp:00003896, author = {新田, 勇 and 坂井, 勇一郎 and 原, 利昭}, issue = {535}, journal = {日本機械学会論文集. C編, 日本機械学会論文集. C編}, month = {Mar}, note = {In a previous paper, it was reported that the shrink fitter was able to improve the fitting strength of the shrink fit between a ceramic shaft and a metal ring at elevated temperature. There are two types of the shrink fitters at present, the monolithic type and the bimetal type. In this paper, the fitting strength of the shrink fitted assemblies using the monolithic shrink fitter or the bimetal one was calculated for two ranges of coefficient of thermal expansion, 0.0~11.7×10^<-6>(/℃) and 18.8~42.5×10^<-6>(/℃). For 18.8~42.5×10^<-6>(/℃), the assembly using the monolithic shrink fitter was stronger than that using the bimetal shrink fitter when the thickness of the shrink fitter in the radial direction was 4mm. The assembly using the bimetal shrink fitter was, however, stronger over approximately 400℃ when the thickness was 1mm. For 0.0~11.7×10^<-6>(/℃), the assembly using the bimetal shrink fitter was stronger over approximately 400℃ regardless of the thickness.}, pages = {985--990}, title = {シュリンクフィッターを用いたセラミックスと金属の締りばめ(種々の熱膨張係数に対する高温結合強度)}, volume = {57}, year = {1991} }