{"_buckets": {"deposit": "be708a20-258d-4847-8aa0-08b0d7966115"}, "_deposit": {"id": "3677", "owners": [], "pid": {"revision_id": 0, "type": "depid", "value": "3677"}, "status": "published"}, "_oai": {"id": "oai:niigata-u.repo.nii.ac.jp:00003677", "sets": ["454", "502"]}, "item_5_alternative_title_1": {"attribute_name": "その他のタイトル", "attribute_value_mlt": [{"subitem_alternative_title": "Residual Stresses and Structure of EB-PVD Thermal Barrier Coatings Exposed at High Temperature"}]}, "item_5_biblio_info_6": {"attribute_name": "書誌情報", "attribute_value_mlt": [{"bibliographicIssueDates": {"bibliographicIssueDate": "2008-03", "bibliographicIssueDateType": "Issued"}, "bibliographicIssueNumber": "739", "bibliographicPageEnd": "376", "bibliographicPageStart": "370", "bibliographicVolumeNumber": "74", "bibliographic_titles": [{"bibliographic_title": "日本機械学会論文集. A編"}, {"bibliographic_title": "日本機械学会論文集. A編", "bibliographic_titleLang": "en"}]}]}, "item_5_description_4": {"attribute_name": "抄録", "attribute_value_mlt": [{"subitem_description": "The substrate material was nickel based superalloy (In738LC), CoNiCrAlY was pressureless plasma-sprayed on the substrate as the bond coating. As the top coating, zirconia with 4 mo1% yittria was made by a electron beam-physical vapor deposition (EB-PVD) with a rotation. The thickness of the bond coating was about 0.18 min, and the thickness of the top coating was about 0.12 mm. The rotation speeds of specimens in the EB-PVD process were 5rpm, 10rpm and 20 rpm. The specimens were exposed at 1273K for 200h. The in-plane residual stress was measured by a conventional X-ray method, and the out-of-plane residual strain was measured by a strain scanning method with hard synchrotron X-rays. For the specimens with 5rpm and 10rpm, the in-plane compressive residual stresses were released by the high temperature exposure. For the specimen with 20 rpm, the in-plane residual stress did not change by the high temperature exposure, because it was very small before the exposure. The in-plane residual stresses were large compression near the interface. For the specimens with 5 rpm and 10 rpm, the out-of plane stresses were small from the coating surface but became a compression near the interface. Both in in-plane and out-of-plane residual stresses of the specimen with 20 rpm were very small. In the effect of decreasing the residual stress, the rotation speed of 20 rpm was the excellent condition. According to the observation with a scanning electron microscope, the feather-like columnar structure decreased after the high temperature exposure. This volume decrease caused the release of the in-plane residual stresses.", "subitem_description_type": "Abstract"}]}, "item_5_full_name_3": {"attribute_name": "著者別名", "attribute_value_mlt": [{"nameIdentifiers": [{"nameIdentifier": "44584", "nameIdentifierScheme": "WEKO"}], "names": [{"name": "Suzuki, Kenji"}]}, {"nameIdentifiers": [{"nameIdentifier": "44585", "nameIdentifierScheme": "WEKO"}], "names": [{"name": "Shobu, Takahisa"}]}, {"nameIdentifiers": [{"nameIdentifier": "44586", "nameIdentifierScheme": "WEKO"}], "names": [{"name": "Wada, Kunihiko"}]}, {"nameIdentifiers": [{"nameIdentifier": "44587", "nameIdentifierScheme": "WEKO"}], "names": [{"name": "Matsubara, Hideaki"}]}]}, "item_5_publisher_7": {"attribute_name": "出版者", "attribute_value_mlt": [{"subitem_publisher": "日本機械学会"}]}, "item_5_select_19": {"attribute_name": "著者版フラグ", "attribute_value_mlt": [{"subitem_select_item": "publisher"}]}, "item_5_source_id_11": {"attribute_name": "書誌レコードID", "attribute_value_mlt": [{"subitem_source_identifier": "AN0018742X", "subitem_source_identifier_type": "NCID"}]}, "item_5_source_id_9": {"attribute_name": "ISSN", "attribute_value_mlt": [{"subitem_source_identifier": "03875008", "subitem_source_identifier_type": "ISSN"}]}, "item_creator": {"attribute_name": "著者", "attribute_type": "creator", "attribute_value_mlt": [{"creatorNames": [{"creatorName": "鈴木, 賢治"}], "nameIdentifiers": [{"nameIdentifier": "44580", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "菖蒲, 敬久"}], "nameIdentifiers": [{"nameIdentifier": "44581", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "和田, 国彦"}], "nameIdentifiers": [{"nameIdentifier": "44582", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "松原, 秀彰"}], "nameIdentifiers": [{"nameIdentifier": "44583", "nameIdentifierScheme": "WEKO"}]}]}, "item_files": {"attribute_name": "ファイル情報", "attribute_type": "file", "attribute_value_mlt": [{"accessrole": "open_date", "date": [{"dateType": "Available", "dateValue": "2019-07-30"}], "displaytype": "detail", "download_preview_message": "", "file_order": 0, "filename": "74-739_370.pdf", "filesize": [{"value": "1.2 MB"}], "format": "application/pdf", "future_date_message": "", "is_thumbnail": false, "licensetype": "license_free", "mimetype": "application/pdf", "size": 1200000.0, "url": {"label": "74-739_370.pdf", "url": "https://niigata-u.repo.nii.ac.jp/record/3677/files/74-739_370.pdf"}, "version_id": "60df584c-3554-43c0-8084-e549e3f1e3fd"}]}, "item_keyword": {"attribute_name": "キーワード", "attribute_value_mlt": [{"subitem_subject": "EB-PVD", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Thermal Barrier Coating", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Residual Stress X-Ray Stress Measurement", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Oxidation", "subitem_subject_scheme": "Other"}]}, "item_language": {"attribute_name": "言語", "attribute_value_mlt": [{"subitem_language": "jpn"}]}, "item_resource_type": {"attribute_name": "資源タイプ", "attribute_value_mlt": [{"resourcetype": "journal article", "resourceuri": "http://purl.org/coar/resource_type/c_6501"}]}, "item_title": "高温暴露されたEB-PVD遮熱コーティングの残留応力と組織", "item_titles": {"attribute_name": "タイトル", "attribute_value_mlt": [{"subitem_title": "高温暴露されたEB-PVD遮熱コーティングの残留応力と組織"}, {"subitem_title": "高温暴露されたEB-PVD遮熱コーティングの残留応力と組織", "subitem_title_language": "en"}]}, "item_type_id": "5", "owner": "1", "path": ["454", "502"], "permalink_uri": "http://hdl.handle.net/10191/18175", "pubdate": {"attribute_name": "公開日", "attribute_value": "2012-06-04"}, "publish_date": "2012-06-04", "publish_status": "0", "recid": "3677", "relation": {}, "relation_version_is_last": true, "title": ["高温暴露されたEB-PVD遮熱コーティングの残留応力と組織"], "weko_shared_id": null}
高温暴露されたEB-PVD遮熱コーティングの残留応力と組織
http://hdl.handle.net/10191/18175
http://hdl.handle.net/10191/18175cb8b6041-053d-4edf-9e39-f958754120b0
名前 / ファイル | ライセンス | アクション |
---|---|---|
74-739_370.pdf (1.2 MB)
|
|
Item type | 学術雑誌論文 / Journal Article(1) | |||||
---|---|---|---|---|---|---|
公開日 | 2012-06-04 | |||||
タイトル | ||||||
タイトル | 高温暴露されたEB-PVD遮熱コーティングの残留応力と組織 | |||||
タイトル | ||||||
言語 | en | |||||
タイトル | 高温暴露されたEB-PVD遮熱コーティングの残留応力と組織 | |||||
言語 | ||||||
言語 | jpn | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | EB-PVD | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | Thermal Barrier Coating | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | Residual Stress X-Ray Stress Measurement | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | Oxidation | |||||
資源タイプ | ||||||
資源 | http://purl.org/coar/resource_type/c_6501 | |||||
タイプ | journal article | |||||
その他のタイトル | ||||||
その他のタイトル | Residual Stresses and Structure of EB-PVD Thermal Barrier Coatings Exposed at High Temperature | |||||
著者 |
鈴木, 賢治
× 鈴木, 賢治× 菖蒲, 敬久× 和田, 国彦× 松原, 秀彰 |
|||||
著者別名 | ||||||
識別子 | 44584 | |||||
識別子Scheme | WEKO | |||||
姓名 | Suzuki, Kenji | |||||
著者別名 | ||||||
識別子 | 44585 | |||||
識別子Scheme | WEKO | |||||
姓名 | Shobu, Takahisa | |||||
著者別名 | ||||||
識別子 | 44586 | |||||
識別子Scheme | WEKO | |||||
姓名 | Wada, Kunihiko | |||||
著者別名 | ||||||
識別子 | 44587 | |||||
識別子Scheme | WEKO | |||||
姓名 | Matsubara, Hideaki | |||||
抄録 | ||||||
内容記述タイプ | Abstract | |||||
内容記述 | The substrate material was nickel based superalloy (In738LC), CoNiCrAlY was pressureless plasma-sprayed on the substrate as the bond coating. As the top coating, zirconia with 4 mo1% yittria was made by a electron beam-physical vapor deposition (EB-PVD) with a rotation. The thickness of the bond coating was about 0.18 min, and the thickness of the top coating was about 0.12 mm. The rotation speeds of specimens in the EB-PVD process were 5rpm, 10rpm and 20 rpm. The specimens were exposed at 1273K for 200h. The in-plane residual stress was measured by a conventional X-ray method, and the out-of-plane residual strain was measured by a strain scanning method with hard synchrotron X-rays. For the specimens with 5rpm and 10rpm, the in-plane compressive residual stresses were released by the high temperature exposure. For the specimen with 20 rpm, the in-plane residual stress did not change by the high temperature exposure, because it was very small before the exposure. The in-plane residual stresses were large compression near the interface. For the specimens with 5 rpm and 10 rpm, the out-of plane stresses were small from the coating surface but became a compression near the interface. Both in in-plane and out-of-plane residual stresses of the specimen with 20 rpm were very small. In the effect of decreasing the residual stress, the rotation speed of 20 rpm was the excellent condition. According to the observation with a scanning electron microscope, the feather-like columnar structure decreased after the high temperature exposure. This volume decrease caused the release of the in-plane residual stresses. | |||||
書誌情報 |
日本機械学会論文集. A編 en : 日本機械学会論文集. A編 巻 74, 号 739, p. 370-376, 発行日 2008-03 |
|||||
出版者 | ||||||
出版者 | 日本機械学会 | |||||
ISSN | ||||||
収録物識別子タイプ | ISSN | |||||
収録物識別子 | 03875008 | |||||
書誌レコードID | ||||||
収録物識別子タイプ | NCID | |||||
収録物識別子 | AN0018742X | |||||
著者版フラグ | ||||||
値 | publisher |